JTB Polymer Cement Waterproof Mortar is a powder product uniformly blended from high-quality cement, quartz sand, imported polymer powder, and a variety of functional additives and admixtures.
• Waterproof, crack & impact resistant
• Reliable high/low temperature & alkali resistance
• Enhances cement mortar bonding
• Customizable formulations
• Eco-friendly
• Exterior walls of buildings,kitchens, bathrooms, balconies, roofs, window perimeters,through-wall pipes & floors,ports, docks, roads & bridges,tanks, water towers, and civil buildings general waterproofing applications
• Surface preparation: The surface of the base layer should be smooth and clean, free of floating dust, grease, dirt and weathered substances, etc. There should be no phenomena such as sanding, hollowing, or cracking. Before construction, it should be rinsed with high-pressure water and kept in a moist state, but there must be no standing water.
• Proportioning and mixing: The water addition should be 18% to 20% of the weight of the JTB polymer cement waterproof mortar. It can be prepared in advance according to the usage. The mixer should be used to stir until the water and materials are fully mixed. Stir until no dry powder remains and the video state is reached.
• Construction: Evenly apply the adhesive slurry on the base layer. The thickness of each application should be between 3mm and 15mm. The reference usage of 3 mm thickness per square meter is 4.5 kg. The initial setting time is 4 hours and the final setting time is 5 to 6 hours.
• Reference dosage: 1.5-2.0KG per square meter.
• Maintenance: After the initial setting of the construction surface, water (spray) maintenance is required. For horizontal ground, it should also be covered with damp gunny bags, etc. Maintenance should be carried out in an environment of 5-40℃.
Packaging specification: Kraft paper-plastic film bags, 25 kg ± 1 kg per bag.
Storage: Store in a well-ventilated and dry place above 5℃, away from direct sunlight. In winter, prevent freezing.
Wear a dust mask, safety goggles, and protective gloves during application.
In case of skin or eye contact, rinse immediately with plenty of clean water. Seek medical treatment promptly if symptoms are severe.
| Inspection items | Performance indicators | Test result | |
| Flexural strength (MPa) | 28d | ≥6 | 7.6 |
| Compressive strength (MPa) | 28d | >18 | 32.1 |
| Bonding strength (MPa) | 7d, MPa | >0.8 | 1.06 |
| Bonding strength (MPa) | 28d, MPa | >1.0 | 1.35 |
| Shrinkage rate (%) | <0.3 | 0.13 | |
| Water absorption rate (%) | <6 | 5.35 | |
JTB technology group are committed to providing customers in all sectors with valuable products and
solutions that offer convenience and efficiency.
Material Science & Construction Water, Stone, and Polymer A close reading of how Polymer-Modified Cementitious Mortar and traditional Lime Mortar behave when water becomes the enemy — and why the answer is rarely as simple as "newer is better." Direct Answer: Polymer-Modif...
READ MORETechnical Engineering Insights Comprehensive Chemical & Mechanical Guide to Concrete Admixtures Modern concrete design relies heavily on chemical formulations to achieve specific performance metrics. Integrating advanced Concrete Admixtures into mix designs allows civil eng...
READ MORETo use concrete repair mortar correctly: remove all loose or crumbling material down to solid concrete, clean and dampen the surface, mix the mortar to a lump-free consistency, apply it in layers no thicker than 20-50mm each, and keep it moist for at least 24-48 hours before all...
READ MORE